Nanoleakage and internal adaptation of zirconia and lithium disilicate single crowns with feather edge preparation

Published: 29 June 2017
Abstract Views: 2073
PDF: 1585
HTML: 100
Publisher's note
All claims expressed in this article are solely those of the authors and do not necessarily represent those of their affiliated organizations, or those of the publisher, the editors and the reviewers. Any product that may be evaluated in this article or claim that may be made by its manufacturer is not guaranteed or endorsed by the publisher.

Authors

Aim The present in vitro study aimed at investigating the nanoleakage and internal adaptation of zirconia and lithium disilicate single crowns with feather edge preparation. Material and Methods Sound mandibular incisors were prepared and randomly divided first into 2 groups, accordingly to restorative materials, and then into 4 subgroups each, in relation to different luting agents. The samples were processed for nanoleakage and then observed for internal adaptation either with a stereomicroscope and a scanning electron microscope. Results The average internal adaptation values were 54.06 μm and 78.66 μm for zirconia and lithium disilicate crowns respectively. The lithium disilicate restorations showed marginal fractures in 39% of the specimens whilst no fractures were observed in the zirconia group. Conclusion Within the limitations of the present in vitro investigation, the feather edge preparation at the cervical margin can be recommended only when zirconia crowns are used.

Dimensions

Altmetric

PlumX Metrics

Downloads

Download data is not yet available.

Citations

How to Cite

Fuzzi, M., Tricarico, M. G., Ferrari Cagidiaco, E., Bonadeo, G., Sorrentino, R., & Ferrari, M. (2017). Nanoleakage and internal adaptation of zirconia and lithium disilicate single crowns with feather edge preparation. Journal of Osseointegration, 9(2), 250–262. https://doi.org/10.23805/jo.2017.09.02.03